304 Stainless Steel Welded Round Tube
Jan 26, 2026
Ostavite poruku



304 Stainless Steel Welded Round Tube is manufactured from high-quality 304 stainless steel using precision welding technology. This austenitic stainless steel tube offers excellent corrosion resistance, superior formability, and outstanding surface finish, making it ideal for structural, decorative, and industrial applications.
Non-magnetic in annealed condition
Cost-effective solution for structural applications
| ASTM A554 Requirement | ||||
|---|---|---|---|---|
| - | 0.080 | 0.045 | <= 0.08 | |
| 18.0 | 20.0 | 18.5 | 18.0-20.0 | |
| 8.0 | 12.0 | 9.2 | 8.0-12.0 | |
| - | 2.00 | 1.45 | <= 2.00 | |
| - | 0.75 | 0.42 | <= 0.75 | |
| - | 0.045 | 0.028 | <= 0.045 | |
| - | 0.030 | 0.015 | <= 0.030 | |
| - | 0.10 | 0.06 | <= 0.10 | |
| 70.1 |