ASME SA 240 SS 317L Cold Rolled Plate
Surface treatment: 2b, Ba, No.1, No.4, Hl, 8K, etc.
Thickness: 0.1mm-300mm or as required
Width: 3mm-2000mm or as required
Delivery time: 7-15 days
Transportation packaging: waterproof paper and steel belt packaging.
HS code: 721921000
Capacity: 8000 tons/year
As a trusted supplier of premium metal materials, GNEE offers a comprehensive range of 317 / 317L stainless steel plates, with all products strictly adhering to international standards such as ASTM, MILS, and AMS. Our core commitment lies in timely delivery and exceptional quality, focusing on providing reliable and cost-effective solutions for our esteemed customers.

ASTM A240 Type 317 stainless steel plates we offer are specifically designed for high-pressure, high-temperature environments and are made from chromium/chromium-nickel alloys. The minimum tensile strength of 317L stainless steel hot-rolled plates reaches 515 MPa, with a minimum yield strength of 205 MPa. These plates are widely used in platforms, storage tanks, transportation equipment, and various high-temperature conditions.
Type 317 stainless steel cold-rolled plates are available in various hardness options, including soft, hard, semi-hard, and spring-hard. Surface finishes include hot-rolled, cold-rolled, and satin. We can also process these plates into coils, foils, strips, or flat sheets. For any inquiries regarding specifications, performance, or pricing, feel free to contact us.
What thicknesses are available for 317/317L alloy steel plates?
We offer 317/317L stainless steel plates in a variety of thicknesses, ranging from 3/16 inch (4.8 mm) to 4 inches (101.6 mm), to meet diverse application requirements.
Thickness: 0.1 mm to 6 mm (sheet), 0.5 mm to 100 mm (plate)
Width: Up to 4200 mm
Length: 2000 mm to 12000 mm (or coiled for sheet)
Surface Finish: Hot-rolled, cold-rolled, annealed, pickled, 2B, No.1, No.4, BA, or customized
Standards: ASTM A240, ASME SA240
Applications: sa 240/a 240 uns s31700 sheets for chemical processing tanks, UNS S31700 plates for pulp and paper equipment
Chemical Composition of Stainless Steel 317L Plates
| C | P | S | |||||||
| SS 317L | 0.035 max | 2.0 max | 1.0 max | 0.045 max | 0.030 max | 18 – 20 | 3 - 4 | 11 – 15 | 57.89 min |
Mechanical Properties of SS 317L Plates
| Yield Strength (0.2%Offset) | ||||
| 7.9 g/cm3 | 1400 ℃ (2550 ℃F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 35 % |
Price List of UNS S31700 Plate
| Price list of Stainless Steel 317 Plate | Stainless Steel 1.4449 Plate Price in USD |
|---|---|
| SS 317L Plate (19.05 X 1.625 X 600mm) | 27.24 USD |
Click to get the most competitive price.
To procure high quality of the Stainless Steel 317L Plates certain parameters are set at each stage of production. Some of the common tests are namely flattering test, mechanical testing, hardness test, the micro and macro test, positive material identification test, pitting resistance test, flaring test, and many more.



ASTM A240 SS 317L Plates Exporter


Packaging: Each sheet or coil is wrapped in moisture-proof paper, lined with plastic film, and secured with steel straps. The outer layer is protected by wooden pallets or crates to ensure safety during international transportation.
Labeling: Each package includes the furnace number, grade, dimensions, and standard information.
Delivery Time: Usually within 7-15 business days after receiving the advance payment.


Popularni tagovi: asme sa 240 ss 317l cold rolled plate, China asme sa 240 ss 317l cold rolled plate manufacturers, suppliers, factory, Boja ploče od nehrđajućeg čelika, Gustoća ploče od nehrđajućeg čelika, tanjur od nehrđajućeg čelika u zabavi, Ploča od nehrđajućeg čelika u hlađenju, Površina ploče od nehrđajućeg čelika, ploča zavarenih od nehrđajućeg čelika